12ga,10ga,8ga,4ga FH;585HE/700HE, other Big Bores--

Picture of fellows at Vestals Gunsmithing test firing 585 HE

they built for a guy. They got 750 gr to almost 2800 from

ultra short barrel, not a full load . A regular barrel would be

over 2900, 14000 ft lbs with full load..

585blast.jpg




Picture of our 375 HE cases, with little 378 WEA on left.

Middle case is with 330 gr, right case is 400gr bullet.

375hecases.jpg



Here is picture of out 375HE testgun, in heavy t-hole stock.

So far 340 gr to 3700 and 360gr 3600.

testgun.jpg



Next 416 HE target case, these run through the hydro-die,

test gun done,will complete testing soon, to confirm specs.

When specs set, info will be sent to reamer guys

Soon will have 408 HE with specs set up also, for guys,

Smaller case 416s and 408s can be reamed out for

our bigger case .Ed

416he.jpg
 
Ed, has anyone built a Pump or Semi-Auto 12 GA FH, with a 3" chamber with any success????? I have a Winchester 1300 and a Benelli M1 Super 90, that both have rifled tube for slug stabilization. That would make a rapid fire super duper thumper if this is possible. Please lend me your thoughts when you get some free time; as well as anyone is more than welcome to comment on the question. Thanks, Jeff
 
For those in plastic we load 600gr slugs with 87 gr 4759

for 1750- 1800 fps, a load that has been lab tested as safe.

With regular thickness slug barrels.ED
 
Here is picture of a brake on 12ga FH with real hot loaded
hollowbase lead slug, brake needed more clearance
for the expanding slug.

bbrake.jpg



Here is the before and after of 375 HE cases
necked, 2 on left, and then formed in hydro die... Ed

beforehydroafter.jpg



Here is pic of 416 HSM second from left we are experimenting
with, going to see if we can make the ultimate 416 ELR case.
Can be 3.60" to 4.00" long, a long one pictured.
Holds over 280 gr ball powder under bullet. The
3.6" case can hold about 250gr under bullet.. In picture,
1st case is 416 HE, 2nd 416 HSM, 3rd 375 He, 4th 378 WEA.

416 HSM will get 400gr to 4100 plus without needing BMG action,
470 gr 3800 plus , it may be the ultimate target, singleshot 416..
Case will work in fat bolt actions, with heavy enough barrel
to have good, milder, barrel harmonics and be under 50 lbs.
A lot of the 2 mile type shoots are adopting 50lb limit.

416hsm.jpg


Here is picture of the 416 HSM fireformed once,
next to bmg case we make it from and as we
improve wildcatting process next few weeks
some specs may make small changes, now from
base to shoulder is 3.45", case 3.97" long. Ed..


hsmbmg.jpg



Manson has 416 HE and 408 HE prints, as well as 375 HE
He can also make you a resize die reamer from that info.
We got 700 cases in 416 and one more pass if 408s wanted, ,
Going to do lot more cases for these 2 sizes,
PM or email. ph 989-644-5228..

Here are final specs for 416 HE.
Length 3.32", belt diameter ,655", base dia .635" ,
length base to to shoulder 2.860" , 30 deg shoulder.Ed
 
Guys asking about strong economical bolt gun to use for 28ga and
410 ga and 32ga with brass cases and higher pressures than plastic cases.
They can use a MN bolt action, here is pic of one with
our 585 case in the action.Guys can get Magtech brass cases or have
RMC make them....Guys can make 32ga case from 500 NE,
410s from 9.3 x 74 brass, etc..

585mosin2.jpg


Here is picture of our 416 HSM case sectioned next to original
BMG case on the right sectioned, to show that we still have
enough thickness in the sides to handle high pressure,
in a case with 310 gr capacity..We are getting the wildcatting
work set up so we can do at least hundred a month.
We have lots of 585s, 375HEs, 416 HEs, 408 HEs.....
And working toward getting 416 HSMs in big numbers.

hsmsect.jpg


Here's comparison of 416 target cases, 1st 416 HE, have whole bunch.
Second is model of what I'd have made on medium machine, if I could,
the 416 HE Long. It has capacity of 230gr..
Third is our 416 HSM which we are working on making by wildcatting bmg
cases, And if had run long cases, make longer 375 HE necking down 416 ..

416heexp.jpg



Bryan Litz just recently shot 3 shot group at 2 miles using Paul
Phillips heavy barreled, target rifle built by Lethal Precision in
375 Lethal Mag(585HE necked down, very similiar to 375HE )...
It grouped 17.5 inches tall by 22 inches wide.

Applied Ballistics shooter Mitch Fitzpatrick just hit 3 of 5 at 3520 yards,
weekend 10-13th at Valdina Ranch , west of San Antonio.
Also used the 375 LM case similar to our 375 HE
Great shooting at the 2017 World's Longest Shot Challenge. Ed
 
The 12ga FH case now is in the new COTW book on
last page in the wildcat section, I think page 324.
They gave good credit to Rob for the idea of that case....


The model 416 HE long case in middle, hydro formed one,

has case capacity of 240 gr, and the 416 HSM in picture,

on the right, we fired a case twice, capacity is 320gr.. Ed..

416heexp.jpg



More info out now; short, fat cases sticking, pockets not lasting as expected.
Trying to get best speeds the things raising pressures are bad case
proportions, too sharp of shoulders, too fast of powders...........
and debth of the bullet into the powder space, as shown in the picture below..
My 375, 416, etc testing, bullets loaded like bottom one, in longer freebore....Ed.

416inout.jpg
 
Here is case measurements for our 416 HE target case
made from our 585 HE big belted case. Ed

416heprint.jpg



Here is picture of 375 HE left, 416 HE next, 416 HSM right..

pat1.jpg



Here, tentative specs, 416 HSM case we are doing from bmg brass,

416hsmpic.jpg




A 375 HE, with Lawton action, bunch being done with those .....

lawton375.jpg
 
Here is recap simple setup to get faster loads with 12ga sabots

& slugs, Example using break actions...., reaming chamber

in a 12ga break action to 3.5" with a 3.5" 12ga reamer, that isn't

something needing special order, and use 3.5" plastic cases , or

get 3.5" brass cases made. With mag shotgun primers and

our slower powder loads you can get a quarter more speed,

which gives 50% more energy...


585 Hubel Express video, 190ft/lbs recoil, heavy load, gun little light.....




Another view of Asteroid Precision's.... 375 HE target gun,

375hehotrod2.jpg



Here is our 416 HSM we are developing next to 416 Barrett, Ed

hsmbarrett.jpg
 
Here in picture of the cases, are shown the steps in making

our 416 HSM case, from BMG brass,, Ed

416process.jpg



We might have a company that is doing a bolt gun with an action

between BMG size and longer rifle actions used for 375 HE,

375 Lethal, and Cheytacs.. To use for our 416 HSM without

having to do extreme rebating of the rim.


Here is picture of 620 416 hsm cases half done. Done on cnc ,

that slimmed them down, cut new rim and extractor groove.

There are over 500 more at cnc getting done now, plus we have

1000s more bmg cases we make them from, when needed..

This case is public domain and if anyone wants to make

them we can give the steps involved...Ed.

hsmcnc.jpg
 
For big long cases our testing is showing that the 416 easier to get powders to work with, less problems ..
Maybe building a target gun,don't have 375 barrel all ready, maybe go 416....

We got cases, 416 HE and 416 HSM, as well as 375...
CEB and others will have bullets...CEB will be doing .416 in 450gr, 475gr, 500gr, 525gr and 550gr

Got sent 5 thick sided sample cases, same OD base as 585/375.416 cases, same belt, just .180" longer,
did a 416 HE, chambered extra barrel , cases stick over 50k. They have about .042" total taper, .021" per
side, when I necked couple to 416. That is a lot of taper , twice the taper of my 416HE...hanging up at 50k..

I could maybe go to 65k with these if we made taper with ..012" - .016" more taper to each side, but that is
no way to build target cases. I'd have to crunch down case shoulder diameter. And would look like 30-30.

And crazy part is, the case has enough brass material to thin up sides and stretch them way out to 4 or
more inches,, They weigh 150 gr more than our 585/375/416,, but with real thick sides they actually
hold less than our 416 HE with thin sides, that is .180" shorter...Our case does 65k ok without sticking..

And we can make super long 4" cases work if we had means to get them built, as we have
15 powders slower than HBMG.Here is pic of thin and thick sided cases, sectioned for comparison.Ed..


thickthin.jpg
 
Here is a drawing depicting the layout of thick and thin sided cases,
like my 585/375/416 HE thin sided ones and the thick one in picture.

And my 585 case is not perfect, as where it transitions from the
heavier corner to the side it isn't gradual, so case separates there
shortening case life. There are others made that way including brand X.
The dotted line is what it should be............

casedrawing.jpg


Others have sent cases to section and look at, that are built thick sided and they
stick also for the folks, If a longer case with about 5 sq in of side surface sticks and
don't spring back, the coefficient of friction is about .01 then the pull needed to move
it is 2500-3500 lbs..That is for big cases with normal amount of slant to the sides.

Here is picture of six nyati and gibbs size cases sectioned..5th one is present 585 HE]
and 6th is thick sided version. 1st is OK which essentially nyati basic case left straight,

allnyati.jpg


In the picture the nyati gma is one we built most of our first 585s on. Before we had factory run.
Reworking made it in size that is my 585 HE, but that brass had the sides of perfect thickness,
not too thick, but thin without sharp transition my new factory 585s had, they last forever as 585s......

Fourth one is an older nyati case I used to make about 10 of my 585s from ...they had thin sides
and sharp transition, and then I tested these 20 years ago, and they would separate after -4-6 hot loads
as 585s, my factory 585 with right powders as a 585 will get 10 hot loads, and necked down to
416/375 4- 6 hot loads, right powders used, Moderate 577 equivalent, factory 585 at least 20 loads..Ed.
 
Guy sent thick sided 375 case, next size base diameter up from Nyati.He said,
'Yes I ran them in a ___________ rifle built by ____, the best I
could get was 44000 psi, any more and they were stuck''

Big bore guys. other forums over the years related that trex/african case in 585
size, thick sided cases, stuck when they loaded them over 45k psi.

Another just sent us, thick sided 375, long case, same base OD as our 585 HE,
416 HE, 375 HE, and Mitch's 375 Lethal, and the thick ones stuck over 45k psi.

Now you can fill those cases up, with ultra slow enough powder so they won't
stick, but powder is too slow for max speed. Might get a little more
speed, with thick sides case, but case got to be 4- 4.5 inches long..

. Anyone needing a sectioned case of the ones I made the first of my 585s from,
contact me, if they want to get a general idea of what case side thickness should
be, in Gibbs size cases on up to about trex and 375 VM size case diameter.

Here is pic of our 585 based case next to brand X and thick ones, both have
same sharp, thinner, corner, where transition from heavy angled corner, to the
side, the carbide draw rod could easily be reshaped with diamond wheel,
just by grinding off sharp transition corner. Then sides would be perfect.., .

brandxthick.jpg



Here is picture of 416 HE in a Choate target/varmint stock guy is doing,
using long action BSA U9 action.Setting in stock ready to do bedding..Ed

choate416he.jpg
 
Warning! This thread is more than 7 years ago old.
It's likely that no further discussion is required, in which case we recommend starting a new thread. If however you feel your response is required you can still do so.
Top